Carbon Content 98.5%
Bulk Density 1.74-1.76 g/cm 3
Thermal Conductivity 0.17-0.21 1050oC W/(m.k)
Electric Resistance 20-25Ωmm 2 /m
Tensile Strength 450-500mpa
Elongation 1.0%
Ash 1.5%
Process Temperature 1450℃
Carbon Content 98.5%
Bulk Density 1.74-1.76 g/cm 3
Thermal Conductivity 0.17-0.21 1050oC W/(m.k)
Electric Resistance 20-25Ωmm 2 /m
Tensile Strength 450-500mpa
Elongation 1.0%
Ash 1.5%
Process Temperature 1450℃